Lord Adhesives 5000 Fast Setting, High Elasticity, Low Viscosity Ethyl Cyanoacrylate Adhesive

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Lord Adhesives
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lord Adhesives 5000 Fast Setting, High Elasticity, Low Viscosity Ethyl Cyanoacrylate Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metals and plastics. Lord Cyanoacrylate Adhesives offer these benefits: Instant Cure. Lord Cyanoacrylate Adhesives develop strong bonds with setting times ranging from 5 to 130 seconds. Ease of Use. Lord Cyanoacrylate Adhesives are one-component systems that facilitate set-up and minimize production costs. Good Environmental Resistance. Lord Cyanoacrylate Adhesives offer excellent resistance to weathering and aging.Lord Adhesives 5000 Fast Setting, High Elasticity, Low Viscosity Ethyl Cyanoacrylate AdhesiveFast setting. High elasticity. Low viscosity. Colorless adhesive for bonding plastic-to-metal and plastic-to-rubber. Very effective in bonding substrates with differing coefficients of expansion. MIL-A-46050C Type II, Class 1 Approved.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0382 lb/in³
Viscosity 30 cP
30 cP
Processing Properties Metric English Comments
Cure Time 0.0333 - 0.0667 min
0.000556 - 0.00111 hour
Plastic set time
0.0333 - 0.0667 min
0.000556 - 0.00111 hour
Rubber set time
0.250 - 0.417 min
0.00417 - 0.00694 hour
Metal set time