Lord Adhesives 8300 Medium Setting, Medium Viscosity Ethyl Cyanoacrylate Adhesive

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Lord Adhesives
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lord Adhesives 8300 Medium Setting, Medium Viscosity Ethyl Cyanoacrylate Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metals and plastics. Lord Cyanoacrylate Adhesives offer these benefits: Instant Cure. Lord Cyanoacrylate Adhesives develop strong bonds with setting times ranging from 5 to 130 seconds. Ease of Use. Lord Cyanoacrylate Adhesives are one-component systems that facilitate set-up and minimize production costs. Good Environmental Resistance. Lord Cyanoacrylate Adhesives offer excellent resistance to weathering and aging.Lord Adhesives 8300 Medium Setting, Medium Viscosity Ethyl Cyanoacrylate AdhesiveMedium setting. Medium viscosity. For bonding O-rings and elastomeric materials. Suitable for bonding more difficult substrates such as EPDM and Viton. Especially helpful for bonding loudspeaker isolator rings. Will qualify for USP Class VI approval. MIL-A-46050C Type II, Class 1 Approved.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Viscosity 20 cP
20 cP
Processing Properties Metric English Comments
Cure Time 0.0167 - 0.0333 min
0.000278 - 0.000556 hour
Rubber set time
0.0333 - 0.0500 min
0.000556 - 0.000833 hour
Plastic set time