Material Notes:
For application on epoxy graphite or other plastic substrates or over a suitable primer on metal.Limitations - Aeroglaze® K3425 primer/surfacer contains no inhibiting pigments and is not suitable in direct-to-metal applications.All information provided by Lord.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
K3425B; ASTM D1475-85
1.54 g/cc
0.0556 lb/in³
Mixed; ASTM D1475-85
1.59 g/cc
0.0574 lb/in³
K3425A; ASTM D1475-85
Solids Content 56.8 %
56.8 %
K3425A; by volume; ASTM D2369-87 Modified
61.1 %
61.1 %
Mixed; by volume; ASTM D2369-87 Modified
75.6 %
75.6 %
K3425A; by weight; ASTM D2369-87 Modified
77.4 %
77.4 %
Mixed; by weight; ASTM D2369-87 Modified
100 %
100 %
K3425B; by weight; ASTM D2369-87 Modified
100 %
100 %
K3425B; by volume; ASTM D2369-87 Modified
Volatile Organic Compounds (VOC) Content 0.00 g/l
0.00 g/l
K3425B; ASTM D3960-87
349 g/l
349 g/l
Mixed; ASTM D3960-87
387 g/l
387 g/l
K3425A; ASTM D3960-87
Brookfield Viscosity 80 cP

@Temperature 25.0 °C
80 cP

@Temperature 77.0 °F
K3425A; RVT, spindle #2 @ 10rpm
200 cP

@Temperature 25.0 °C
200 cP

@Temperature 77.0 °F
Mixed; RVT, spindle #2 @ 10rpm
2100 cP

@Temperature 25.0 °C
2100 cP

@Temperature 77.0 °F
K3425B; RVT, spindle #2 @ 10rpm
Thermal Properties Metric English Comments
Flash Point 26.7 °C
80.1 °F
K3425A; Setaflash, Closed Cup; ASTM D3278-82
>= 93.0 °C
>= 199 °F
K3425B; Setaflash, Closed Cup; ASTM D3278-82
Processing Properties Metric English Comments
Cure Time 360 min

@Temperature 25.0 °C
6.00 hour

@Temperature 77.0 °F
50% relative humidity
Pot Life 240 min

@Temperature 25.0 °C
240 min

@Temperature 77.0 °F
50% relative humidity
Shelf Life 12.0 Month

@Temperature 25.0 °C
12.0 Month

@Temperature 77.0 °F
50% relative humidity
Descriptive Properties Value Comments
Appearance Gray
Coating Film Dry Weight (gm/ft²/mil) 4.61
Theoretical Coverage (ft²/gallon/mil) 980