Lord Adhesives Fusor® 2200 / 2201 Urethane Adhesive

Category Polymer , Adhesive
Manufacturer Lord Adhesives
Trade Name Fusor®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lord Adhesives Fusor® 2200 / 2201 Urethane Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fusor® 2200/2201 is a black equal-mix, twocomponent, paste urethane adhesive system. Fusor 2200/2201 adhesive bonds FRP, SMC, and other plastics with little surface preparation where bond strengths greater than the substrate are desired. This adhesive also bonds primed metals and various combinations of dissimilar substrates. Fusor 2200/2201 adhesive system is available in a range of working times to accommodate a wide variety of process requirements.All information provided by Lord.
Physical Properties Metric English Comments
Density 1.30 - 1.34 g/cc
0.0470 - 0.0484 lb/in³
Fusor 2201
1.50 - 1.53 g/cc
0.0542 - 0.0553 lb/in³
Fusor 2200
Solids Content 99.5 %
99.5 %
Fusor 2200
100 %
100 %
Fusor 2201
Brookfield Viscosity 25000 - 70000 cP

@Temperature 25.0 °C
25000 - 70000 cP

@Temperature 77.0 °F
Fusor 2200
230000 - 530000 cP

@Temperature 25.0 °C
230000 - 530000 cP

@Temperature 77.0 °F
Fusor 2201
Thermal Properties Metric English Comments
Flash Point >= 93.0 °C
>= 199 °F
Fusor 2200; Closed Cup
>= 93.0 °C
>= 199 °F
Fusor 2201; Closed Cup
Processing Properties Metric English Comments
Cure Time 1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Shelf Life 6.00 Month

@Temperature 18.0 - 29.0 °C
6.00 Month

@Temperature 64.4 - 84.2 °F
Descriptive Properties Value Comments
Appearance Black
Fusor 2201
Brown
Fusor 2200
Consistency Paste
Fusor 2200
Paste
Fusor 2201
Mix Ratio 1:.87
by weight
1:1
by volume