Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lotte Chemical Titan TITANEX® MR4086 Medium density polyethylene resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Rotational Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lotte Chemical Titan TITANEX® MR4086 Medium density polyethylene resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MR4086 is a UV stabilized, pelleted medium density polyethylene for rotomolding.Applications: Large industrial tanks, agriculture tanks, chemical drums, bins, cones, bottle caps.Advantages: Excellent stress crack resistance, high modulus at equal density, excellent dimension stability, better low temperature impact strength, broad molding latitude.Information provided by Titan Chemicals
Physical Properties Metric English Comments
Base Resin Density 0.938 g/cc
0.0339 lb/in³
ASTM D1505
ESCR 100% Igepal® >= 1000 hour

@Thickness 3.18 mm
>= 1000 hour

@Thickness 0.125 in
bent strip, non slit; ASTM D1693
Base Resin Melt Index 4.0 g/10 min
4.0 g/10 min
I<sub>2</sub>; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 17.7 MPa
2570 psi
ASTM D638
Elongation at Break >= 660 %
>= 660 %
ASTM D638
Flexural Modulus 0.892 GPa
129 ksi
ASTM D790
1% Secant Modulus 568.78 MPa
82495 psi
ASTM D638
Thermal Properties Metric English Comments
Vicat Softening Point 117 °C
243 °F
resin; ASTM D1525