Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lotte Chemical Titan TITANPRO® PM803 Polypropylene homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Lotte Chemical Titan Holding Sdn. Bhd. (Former Titan Chemicals)
Trade Name TITANPRO®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lotte Chemical Titan TITANPRO® PM803 Polypropylene homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Titanpro® PM803 is a high flow and also a controlled rheology grade. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 177.1520(b). In summary, this resin meets the FDA criteria covering safe use of polyolefin articles and component of articles intended for food contact use. Applications: Thin walled injection molding (TWIM) articles. Disposable containers and lids, party plates, pen barrels.Advantages: Low molded in stress. Good clarity. Good balance of stiffness and impact strength. Specifically designed for short cycle time. Low warpage.Fabrication: Equipment - ram or screw injection machines. Techniques - standard processing. Information provided by Titan ChemicalsCAS# 9003-07-0
Physical Properties Metric English Comments
Base Resin Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Water Absorption 0.020 %
0.020 %
after 24 hrs; ASTM D570
Base Resin Melt Index 50 g/10 min

@Temperature 230 °C
50 g/10 min

@Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 108
108
ASTM D785A
Tensile Strength, Yield 34.3 MPa
4970 psi
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus 1.77 GPa
257 ksi
ASTM D790B
Izod Impact, Notched 0.196 J/cm
0.367 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C
248 °F
ASTM D648