Lotte Chemical Titan TITANZEX® HB6200 High density polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Lotte Chemical Titan Holding Sdn. Bhd. (Former Titan Chemicals)
Trade Name TITANZEX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lotte Chemical Titan TITANZEX® HB6200 High density polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HB6200 is a high density polyethylene for blow molding. HB6200 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1a & 3.2a. Applications: Household and industrial chemical containers Toiletries Cosmetic containers Pharmaceutical containersAdvantages: Excellent ESCR Excellent mechanical strengthInformation provided by Titan Chemicals
Physical Properties Metric English Comments
Base Resin Density 0.956 g/cc
0.0345 lb/in³
ASTM D1505
Environmental Stress Crack Resistance >= 600 hour
>= 600 hour
F<sub>50</sub>; ASTM D1693
Base Resin Melt Index 0.45 g/10 min
0.45 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
ASTM D2240
Tensile Strength at Break 34.3 MPa
4970 psi
ASTM D638
Tensile Strength, Yield 26.5 MPa
3840 psi
ASTM D638
Elongation at Break >= 500 %
>= 500 %
ASTM D638
Flexural Stiffness 980.7 MPa
142200 psi
Olsen; ASTM D747
Izod Impact, Notched 0.980 J/cm
1.84 ft-lb/in
ASTM D256