Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lotte Chemical Titan TITANZEX® HI2200 High density polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Lotte Chemical Titan Holding Sdn. Bhd. (Former Titan Chemicals)
Trade Name TITANZEX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lotte Chemical Titan TITANZEX® HI2200 High density polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HI2200 is a high density polyethylene for injection molding. HI2200 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1a & 3.2a.Applications: Large sized heavy duty articles Crates and containers Industrial pails Chicken cages DustbinsAdvantages: Excellent mechanical strengthInformation provided by Titan Chemicals
Physical Properties Metric English Comments
Base Resin Density 0.957 g/cc
0.0346 lb/in³
ASTM D1505
Environmental Stress Crack Resistance 5.0 hour
5.0 hour
F<sub>50</sub>; ASTM D1693
Base Resin Melt Index 4.0 g/10 min
4.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
ASTM D2240
Tensile Strength at Break 16.7 MPa
2420 psi
ASTM D638
Tensile Strength, Yield 32.4 MPa
4700 psi
ASTM D638
Elongation at Break >= 300 %
>= 300 %
ASTM D638
Flexural Stiffness 1030 MPa
149300 psi
Olsen; ASTM D747
Izod Impact, Notched 0.588 J/cm
1.10 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 124 °C
255 °F
resin; ASTM D1525
Users viewing this material also viewed the following: