Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Loxim 235 01V0 Polybutylene Terephthalate

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled , Polybutylene Terephthalate (PBT), Flame Retardant
Manufacturer Loxim Industries
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loxim 235 01V0 Polybutylene Terephthalate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Loxim Industries
Physical Properties Metric English Comments
Specific Gravity 1.67 - 1.71 g/cc
1.67 - 1.71 g/cc
ASTM D792
Filler Content 35 %
35 %
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
ASTM D1299
Mechanical Properties Metric English Comments
Tensile Strength at Break 130 MPa
18900 psi
ASTM D683
Elongation at Break 4.0 %
4.0 %
ASTM D638
Tensile Modulus 9.00 GPa
1310 ksi
ASTM D638
Flexural Modulus 9.50 GPa
1380 ksi
ASTM D790
Izod Impact, Notched 0.600 - 0.650 J/cm
1.12 - 1.22 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 215 - 225 °C
419 - 437 °F
ASTM D1525, HDT Method B
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in