Material Notes:
These diester-based synthetic air compressor fluids are outstanding for applications where the fluid is subjected to high temperature and high stress conditions over extended drain intervals.Synac Series Fluids are available in Pails & Drums.Information provided by Lubriplate
Physical Properties Metric English Comments
Viscosity Measurement 77
77
Viscosity Index
320
320
ISO Grade
Saybolt Viscosity at 100°F 1496 SUS
1496 SUS
Saybolt Viscosity at 210°F 99 SUS
99 SUS
Kinematic Viscosity at 40°C (104°F) 290 cSt
290 cSt
Kinematic Viscosity at 100°C (212°F) 20 cSt
20 cSt
Thermal Properties Metric English Comments
Pour Point -20.6 °C
-5.00 °F
Flammability Test 505
505
[°F] Fire Point
Flash Point 246 °C
475 °F