Lubrizol Advanced Materials PEARLCOAT® 126K Thermoplastic Polyurethane Elastomer  (discontinued **)

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials PEARLCOAT® 126K Thermoplastic Polyurethane Elastomer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PEARLCOAT® 126K is a polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low temperature flexibility and medium softening point. PEARLCOAT® 126K is used in melt coatings on textile substrates, for conveyor belts, belting, among other end uses, obtained by extrusion, calendering or sintering (in this last case the product is previously ground, so as to be in powder form). PEARLCOAT® 126K is used for obtaining extruded films and fabric coatings.All information provided by Merquinsa
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Melt Flow 10 g/10 min

@Load 21.6 kg
10 g/10 min

@Load 47.6 lb
Mechanical Properties Metric English Comments
Hardness, Shore A 94
94
ASTM D2240
Tensile Strength, Yield 35.00 MPa
5076 psi
ASTM D412
Elongation at Break 420 %
420 %
ASTM D412
100% Modulus 0.01302 GPa
1.889 ksi
ASTM D412
300% Modulus 0.02504 GPa
3.632 ksi
ASTM D412
Abrasion 40
40
loss (mm³); DIN 53.516
Thermal Properties Metric English Comments
Melting Point 155 - 165 °C
311 - 329 °F
MQSA 111
Glass Transition Temp, Tg -22.2 °C
-8.00 °F
DSC, 10ºC/min; DIN 51.007
Processing Properties Metric English Comments
Zone 1 150 - 160 °C
302 - 320 °F
Zone 2 160 - 170 °C
320 - 338 °F
Zone 3 170 - 180 °C
338 - 356 °F
Zone 4 175 - 185 °C
347 - 365 °F
Die Temperature 175 - 185 °C
347 - 365 °F
Moisture Content <= 0.10 %
<= 0.10 %
MQSA 44