Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Advanced Materials PEARLCOAT® Activa D126K BL Thermoplastic Polyurethane Elastomer  (discontinued **)

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials PEARLCOAT® Activa D126K BL Thermoplastic Polyurethane Elastomer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PEARLCOAT® Activa D126K BL is a standard polyester based TPU, supplied in form of translucent, black colored pellets, combining hardness with excellent low-temperature flexibility. PEARLCOAT® Activa D126K BL is used in melt coatings on textile substrates for conveyor belts obtained by sintering (in this case the product is previously ground, so as to be in powder form). For optimum results, previous drying of the product during 2 hours at 194-212º F is advisable, in a hot air circulatory, vacuum or desiccant-air dryer.All information provided by Merquinsa
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
Melt Flow 10 g/10 min

@Load 21.6 kg
10 g/10 min

@Load 47.6 lb
Mechanical Properties Metric English Comments
Hardness, Shore A 94
94
ASTM D2240
Tensile Strength, Yield 35.06 MPa
5085 psi
ASTM D412
Elongation at Break 450 %
450 %
ASTM D412
100% Modulus 0.0170 GPa
2.47 ksi
ASTM D412
300% Modulus 0.02905 GPa
4.214 ksi
ASTM D412
Abrasion 50
50
loss (mm³); DIN 53.516
Thermal Properties Metric English Comments
Melting Point 154 - 166 °C
310 - 330 °F
MQSA 111
Glass Transition Temp, Tg -22.8 °C
-9.00 °F
DSC, 10ºC/min; DIN 51.007