Lubrizol Advanced Materials PEARLTHANE® 11T93 Thermoplastic Polyurethane Elastomer

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Lubrizol Advanced Materials Manufacturing S. S.L. (Former Merquinsa)
Trade Name Pearlthane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials PEARLTHANE® 11T93 Thermoplastic Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type : Pearlthane® 11T93 is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining hardness with excellent mechanical properties, including a low compression set value.All information provided by Merquinsa
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ISO 2781
Mechanical Properties Metric English Comments
Hardness, Shore A 93
93
ISO 868
Tensile Strength, Yield 40.00 MPa
5801 psi
ISO 527-2/5A/500
Elongation at Break 500 %
500 %
ISO 527-2/5A/500
50% Modulus 0.0700 GPa
10.2 ksi
ISO 527-2/5A/500
100% Modulus 0.008998 GPa
1.305 ksi
ISO 527-2/5A/500
300% Modulus 0.01700 GPa
2.465 ksi
ISO 527-2/5A/500
Tear Strength 120 kN/m
685 pli
ISO 34-1B
Abrasion 25
25
loss (mm³); ISO 4649-A
Thermal Properties Metric English Comments
Vicat Softening Point 102 °C
216 °F
ISO 306
Processing Properties Metric English Comments
Feed Temperature 40.0 °C
104 °F
Nozzle Temperature 210 °C
410 °F
Zone 1 195 °C
383 °F
Zone 2 200 °C
392 °F
Zone 3 210 °C
410 °F
Zone 4 210 °C
410 °F