Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Advanced Materials PEARLTHANE® 16N85UV Thermoplastic Polyurethane Elastomer  (discontinued **)

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials PEARLTHANE® 16N85UV Thermoplastic Polyurethane Elastomer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PEARLTHANE® 16N85UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of translucent, colorless, combining hardness with excellent mechanical properties and excellent hydrolysis resistance. It can be extruded and injection-molded. PEARLTHANE® 16N85UV when extruded, is used for making films, cables, tubing and profiles. When processed by injection molding, it can be used for making technical parts.All information provided by Merquinsa
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ASTM D792
Melt Flow 10 g/10 min

@Load 21.6 kg
10 g/10 min

@Load 47.6 lb
Mechanical Properties Metric English Comments
Hardness, Shore A 87
87
ASTM D2240
Tensile Strength 33.79 MPa
4901 psi
ASTM D-412
Elongation at Break 570 %
570 %
ASTM D412
100% Modulus 0.00600 GPa
0.870 ksi
ASTM D412
300% Modulus 0.01100 GPa
1.595 ksi
ASTM D412
Tear Strength 90.3 kN/m
515 pli
ASTM D624 (Die C)
Abrasion 25
25
loss (mm³); DIN 53.516
Compression Set 24 %

@Temperature 23.0 °C,
Time 252000 sec
24 %

@Temperature 73.4 °F,
Time 70.0 hour
ASTM D395B
35 %

@Temperature 70.0 °C,
Time 86400 sec
35 %

@Temperature 158 °F,
Time 24.0 hour
ASTM D395B
Thermal Properties Metric English Comments
Melting Point 171 - 181 °C
340 - 358 °F
MQSA 111
Glass Transition Temp, Tg -47.8 °C
-54.0 °F
DSC, 18ºF/min; DIN 51.007
Processing Properties Metric English Comments
Feed Temperature 195 °C
383 °F
Nozzle Temperature 200 °C
392 °F
Zone 1 185 - 200 °C
365 - 392 °F
Zone 2 200 - 230 °C
392 - 446 °F
Zone 3 210 - 230 °C
410 - 446 °F
Zone 4 200 - 220 °C
392 - 428 °F
Die Temperature 190 - 195 °C
374 - 383 °F
Mold Temperature 35.0 °C
95.0 °F
Moisture Content <= 0.10 %
<= 0.10 %
MQSA 44
Screw Speed 50 rpm
50 rpm
Copyright © lookpolymers.com All Rights Reserved