Lubrizol Advanced Materials PEARLTHANE® 18VT80 Thermoplastic Polyurethane Elastomer  (discontinued **)

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials PEARLTHANE® 18VT80 Thermoplastic Polyurethane Elastomer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PEARLTHANE® 18VT80 is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and superior hydrolysis and microbe resistance. PEARLTHANE® 18VT80 features a high moisture vapor transmission. PEARLTHANE® 18VT80 can be used for blown- and cast films for a wide variety of applications such as textile lamination. In addition, specific masterbatches for thin films are available. We strongly recommend the use of Pearlthane® MB52BK to ease the processing of this grade.All information provided by Merquinsa
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Water Vapor Transmission 8000 g/m²/day
515 g/100 in²/day
38%, 90%RH; DIN 53.122
Melt Flow 10 g/10 min

@Load 21.6 kg
10 g/10 min

@Load 47.6 lb
Mechanical Properties Metric English Comments
Hardness, Shore A 81
81
ASTM D2240
Tensile Strength, Yield 30.05 MPa
4359 psi
ASTM D412
Elongation at Break 670 %
670 %
ASTM D412
100% Modulus 0.00501 GPa
0.726 ksi
ASTM D412
300% Modulus 0.009018 GPa
1.308 ksi
ASTM D412
Tear Strength 75.4 kN/m
430 pli
ASTM D624 (Die C)
Abrasion 44
44
loss (mm³); DIN 53.516
Thermal Properties Metric English Comments
Melting Point 173 - 183 °C
343 - 361 °F
MQSA 111
Glass Transition Temp, Tg -31.1 °C
-24.0 °F
DSC, 18ºF/min; DIN 51.007