Lubrizol Advanced Materials Pearlbond® 12C75 Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Lubrizol Advanced Materials Manufacturing S. S.L. (Former Merquinsa)
Trade Name Pearlbond®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials Pearlbond® 12C75 Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Pearlbond® 12C75 is polyester-based thermoplastic polyurethane, supplied in form of colourless, translucent granules, combining hardness with excellent low-temperature flexibility and a low softening point.APPLICATIONS: Pearlbond® 12C75 is mainly used for making heat-sealable fabrics (thermobonding), obtained by coating processes such as:Hot Melt Coating system: Rotogravure hot melt printing. The product is melted in an extruder and then pumped into a deposit in front of the engraved roller.Powder Coating system: Scattering or dot-coating (powder or paste). The product is previously ground into powder, by cryogenic grinding. The particle size of the powder will depend on the application technique to be used.
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ISO 2781
Viscosity 1.05e+6 cP

@Temperature 160 °C
1.05e+6 cP

@Temperature 320 °F
Melt; ISO 1133
Melt Flow 15 - 40 g/10 min

@Load 2.16 kg,
Temperature 170 °C
15 - 40 g/10 min

@Load 4.76 lb,
Temperature 338 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 78
78
ISO 868
Tensile Strength at Break 24.0 MPa
3480 psi
ISO 527
Elongation at Break 650 %
650 %
ISO 527
100% Modulus 0.00400 GPa
0.580 ksi
ISO 527
300% Modulus 0.00500 GPa
0.725 ksi
ISO 527
Thermal Properties Metric English Comments
Melting Point 130 - 140 °C
266 - 284 °F
MQSA 70 A
Softening Point 110 - 130 °C
230 - 266 °F
MQSA 70 A
Processing Properties Metric English Comments
Zone 1 120 - 130 °C
248 - 266 °F
Zone 2 130 - 140 °C
266 - 284 °F
Zone 3 140 - 150 °C
284 - 302 °F
Zone 4 145 - 155 °C
293 - 311 °F
Die Temperature 145 - 155 °C
293 - 311 °F