Lubrizol Advanced Materials Pearlbond® 539 Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Lubrizol Advanced Materials Manufacturing S. S.L. (Former Merquinsa)
Trade Name Pearlbond®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials Pearlbond® 539 Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Pearlbond® 539 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a very high thermoplasticity level.Application: Pearlbond® 539 can be added to formulations of REACTIVE POLYURETHANE HOT-MELTS (HMPUR), in order to improve the crystallisation speed.Information provided by Merquinsa
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ISO 2781
Viscosity 1.70e+6 cP

@Temperature 130 °C
1.70e+6 cP

@Temperature 266 °F
Melt; ISO 1133
Melt Flow 150 - 200 g/10 min

@Load 2.16 kg,
Temperature 170 °C
150 - 200 g/10 min

@Load 4.76 lb,
Temperature 338 °F
ISO 1133
Thermal Properties Metric English Comments
Melting Point 58.0 - 60.0 °C
136 - 140 °F
MQSA 70A
Processing Properties Metric English Comments
Moisture Content <= 0.15 %
<= 0.15 %
MQSA 44
Descriptive Properties Value Comments
Crystallization Rate 8-10 minutes
OH Value < 5 mg KOH/g.
MQSA 47A
Thermoplasticity Level Very Low