Lubrizol Advanced Materials Pearlthane® D16N60D Thermoplastic Polyurethane Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Polyester Grade
Manufacturer Lubrizol Advanced Materials Manufacturing S. S.L. (Former Merquinsa)
Trade Name Pearlthane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials Pearlthane® D16N60D Thermoplastic Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type : Pearlthane® 16N60D is a polyether-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining high hardness with excellent mechanical properties and good hydrolysis and microbial resistance.Information provided by Merquinsa.
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ISO 2781
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ISO 868
Tensile Strength, Yield 40.00 MPa
5802 psi
ISO 527-2/5A/500
Elongation at Break 400 %
400 %
ISO 527-2/5A/500
50% Modulus 0.0140 GPa
2.03 ksi
ISO 527-2/5A/500
100% Modulus 0.0190 GPa
2.76 ksi
ISO 527-2/5A/500
300% Modulus 0.0340 GPa
4.93 ksi
ISO 527-2/5A/500
Tear Strength 190 kN/m
1080 pli
ISO 34-1B
Thermal Properties Metric English Comments
Vicat Softening Point 110 °C
230 °F
ISO 306
Processing Properties Metric English Comments
Feed Temperature 40.0 °C
104 °F
Nozzle Temperature 210 °C
410 °F
Zone 1 205 °C
401 °F
Zone 2 210 °C
410 °F
Zone 3 215 °C
419 °F
Zone 4 215 °C
419 °F
Dry Time 3.00 hour

@Temperature 100 °C
3.00 hour

@Temperature 212 °F