Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Advanced Materials Pearlthane® MB-9005 Thermoplastic Polyurethane Elastomer

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Lubrizol Advanced Materials Manufacturing S. S.L. (Former Merquinsa)
Trade Name Pearlthane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials Pearlthane® MB-9005 Thermoplastic Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Pearlthane® MB-9005 is a TPU-based color masterbatch, supplied in the form of homogenously black colored pellets. It is specially intended for coloring TPUs (either polyester or polyether-based), for extrusion, injection molding or calendering processes.Applications:Pearlthane MB-9005 can be mixed with any items of Merquinsa's Pearlthane or Pearlcoat lines (either polyester or polyether-based) intended for applications obtained by extrusion, injection molding or calendering.A 2% usage level (on TPU, by weight) is recommended. Higher levels can be considered, depending on the requirements of the end-product. A good color consistency requires an accurate dosing and good distribution in the TPU.
Physical Properties Metric English Comments
Apparent Bulk Density 0.700 g/cc
0.0253 lb/in³
ASTM D-1875
Component Elements Properties Metric English Comments
Carbon, C 40 %
40 %
Processing Properties Metric English Comments
Processing Temperature <= 240 °C
<= 464 °F
Drying Temperature 100 - 110 °C

@Time 3600 - 7200 sec
212 - 230 °F

@Time 1.00 - 2.00 hour
In hot air circulatory, vacuum, or desiccant-air dryer
Descriptive Properties Value Comments
Colour Index n0 RAL 9005
Lightfastness 8
(1-8) Scale of blue tones; DIN 53 389
Users viewing this material also viewed the following: