Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol ESTANE® 58091 Ester Based Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Polyester Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® 58091 Ester Based Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: High stiffness TPU alloyUses: Flat Die/Cast Sheet Extrusion, Profile Extrusion and Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ASTM D792
Maximum Moisture Content 0.020
0.020
Mechanical Properties Metric English Comments
Hardness, Shore D 67 - 73

@Time 15.0 sec
67 - 73

@Time 0.00417 hour
ASTM D2240
Tensile Strength 29.0 MPa
4210 psi
ASTM D412
Elongation at Break 160 %
160 %
ASTM D412
100% Modulus 0.0283 GPa
4.10 ksi
ASTM D412
Flexural Modulus 0.441 GPa
64.0 ksi
ASTM D790
Graves Tear Strength 193 kN/m
1100 pli
Die C; ASTM D624
Thermal Properties Metric English Comments
Melting Point 106 °C
223 °F
ASTM D1525
Glass Transition Temp, Tg -11.0 °C
12.2 °F
DSC
Processing Properties Metric English Comments
Zone 1 188 °C
370 °F
Extrusion
Zone 2 194 °C
381 °F
Extrusion
Zone 3 199 °C
390 °F
Extrusion
Zone 4 205 °C
401 °F
Extrusion
Adapter Temperature 205 °C
401 °F
5, Extrusion
Die Temperature 205 °C
401 °F
Zone 1, Extrusion
205 °C
401 °F
Zone 2, Extrusion
Drying Temperature 104 °C
219 °F
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Dew Point -40.0 °C
-40.0 °F
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved