Lubrizol ESTANE® 58202 Ether Based Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Ether Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® 58202 Ether Based Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Halogenated flame retardant compound with good low temperature properties and cut resistanceUses: Extrusion – wire and cable jacketing and general extrusion where flame retardant propertied are required.Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
Loss On Ignition 32 %
32 %
ASTM D2863
Maximum Moisture Content 0.020
0.020
Mechanical Properties Metric English Comments
Hardness, Shore A 82 - 88

@Time 5.00 sec
82 - 88

@Time 0.00139 hour
ASTM D2240
Tensile Strength 27.6 MPa
4000 psi
ASTM D412
Elongation at Break 650 %
650 %
ASTM D412/D638
100% Modulus 0.00550 GPa
0.798 ksi
ASTM D412
300% Modulus 0.00190 GPa
0.276 ksi
ASTM D412
Tear Strength 18.4 kN/m
105 pli
Trouser; ASTM D470
Graves Tear Strength 63.1 kN/m
360 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 155
155
H-18, 1000g; ASTM D3389 B
Thermal Properties Metric English Comments
Melting Point 115 °C
239 °F
DSC
Glass Transition Temp, Tg -45.0 °C
-49.0 °F
DSC
Flammability Test 5.0
5.0
Processing Properties Metric English Comments
Zone 1 174 °C
345 °F
Extrusion
Zone 2 179 °C
354 °F
Extrusion
Zone 3 185 °C
365 °F
Extrusion
Zone 4 188 °C
370 °F
Extrusion
Adapter Temperature 188 °C
370 °F
5, Extrusion
Die Temperature 188 °C
370 °F
Zone 1, 6, Extrusion
188 °C
370 °F
Zone 2, Extrusion
Drying Temperature 104 °C
219 °F
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Dew Point -40.0 °C
-40.0 °F