Lubrizol ESTANE® 58244 Ether Based Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Ether Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® 58244 Ether Based Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Non-Halogenated flame retardant compoundUses: Extrusion – wire and cable and general extrusion where flame retardant propertied are requiredAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM D792
Loss On Ignition 28 %
28 %
ASTM D2863
Maximum Moisture Content 0.020
0.020
Mechanical Properties Metric English Comments
Hardness, Shore A 87 - 93

@Time 5.00 sec
87 - 93

@Time 0.00139 hour
ASTM D2240
Tensile Strength 13.8 MPa
2000 psi
ASTM D412
Elongation at Break 640 %
640 %
ASTM D412
100% Modulus 0.00690 GPa
1.00 ksi
ASTM D412
300% Modulus 0.00760 GPa
1.10 ksi
ASTM D412
Tear Strength 193 kN/m
1100 pli
Trouser; ASTM D470
Graves Tear Strength 175 kN/m
1000 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 350
350
H18, 1000g; ASTM D3389
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
Processing Properties Metric English Comments
Zone 1 182 °C
360 °F
Extrusion
Zone 2 188 °C
370 °F
Extrusion
Zone 3 194 °C
381 °F
Extrusion
Zone 4 196 °C
385 °F
Extrusion
Adapter Temperature 196 °C
385 °F
Extrusion
Die Temperature 188 °C
370 °F
Zone 2, Extrusion
194 °C
381 °F
Zone 1, Extrusion
Drying Temperature 104 °C
219 °F
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Dew Point -40.0 °C
-40.0 °F
Descriptive Properties Value Comments
Smoke Index 24
NES 711