Lubrizol ESTANE® 58325 Ether Based Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Ether Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® 58325 Ether Based Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: High melt strength for thick sheet extrusion.Uses: Blown and Flat Die/Cast Extrusion, Tubing and Profile ExtrusionAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ASTM D792
Maximum Moisture Content 0.020
0.020
Mechanical Properties Metric English Comments
Hardness, Shore A 82 - 88

@Time 5.00 sec
82 - 88

@Time 0.00139 hour
ASTM D2240
Tensile Strength 51.7 MPa
7500 psi
ASTM D412
Elongation at Break 615 %
615 %
ASTM D412
100% Modulus 0.00550 GPa
0.798 ksi
ASTM D412
300% Modulus 0.00970 GPa
1.41 ksi
ASTM D412
Flexural Modulus 0.0277 GPa
4.02 ksi
ASTM D790
Tear Strength 24.5 kN/m
140 pli
Trouser; ASTM D470
Graves Tear Strength 78.9 kN/m
450 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 63
63
H18, 1000g; ASTM D3389 B
Tensile Set 10 %
10 %
200% elongation; ASTM D412
Thermal Properties Metric English Comments
Melting Point 131 °C
268 °F
DSC
Glass Transition Temp, Tg -44.0 °C
-47.2 °F
DSC
Processing Properties Metric English Comments
Zone 1 183 °C
361 °F
Extrusion
Zone 2 188 °C
370 °F
Extrusion
Zone 3 194 °C
381 °F
Extrusion
Zone 4 199 °C
390 °F
Extrusion
Adapter Temperature 199 °C
390 °F
Extrusion
Die Temperature 199 °C
390 °F
Zone 1, Extrusion
199 °C
390 °F
Zone 2, Extrusion
Drying Temperature 104 °C
219 °F
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Dew Point -40.0 °C
-40.0 °F