Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol ESTANE® 58630 Ether Based Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Ether Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® 58630 Ether Based Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Good physical properties, hydrolysis resistance, low temperature performance and abrasion along with wide processing window for extrusion and low surface tack.Uses: Blown and flat die/cast film extrusion and cable jacketing.Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Maximum Moisture Content 0.020
0.020
Mechanical Properties Metric English Comments
Hardness, Shore A 79 - 85

@Time 5.00 sec
79 - 85

@Time 0.00139 hour
ASTM D2240
Tensile Strength 41.4 MPa
6000 psi
ASTM D412
Elongation at Break 640 %
640 %
ASTM D412/D638
100% Modulus 0.00520 GPa
0.754 ksi
ASTM D412
300% Modulus 0.00760 GPa
1.10 ksi
ASTM D412
Tear Strength 22.8 kN/m
130 pli
Trouser; ASTM D470
Graves Tear Strength 70.1 kN/m
400 pli
DIe C; ASTM D624
Taber Abrasion, mg/1000 Cycles 60
60
H18, 1000g; ASTM D3389 B
Tensile Set 15 %
15 %
200% elongation; ASTM D412
Thermal Properties Metric English Comments
Melting Point 120 °C
248 °F
DSC
125 °C
257 °F
Kofler
Glass Transition Temp, Tg -50.0 °C
-58.0 °F
DSC
Processing Properties Metric English Comments
Zone 1 166 °C
331 °F
Extrusion
Zone 2 171 °C
340 °F
Extrusion
Zone 3 177 °C
351 °F
Extrusion
Zone 4 182 °C
360 °F
Extrusion
Adapter Temperature 182 °C
360 °F
5, Extrusion
Die Temperature 182 °C
360 °F
6, Zone 1, Extrusion
182 °C
360 °F
Zone 2, Extrusion
Drying Temperature 104 °C
219 °F
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Dew Point -40.0 °C
-40.0 °F
Descriptive Properties Value Comments
Volume Swell in Water 2.1%
24h, 23°C; ASTM D471