Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol ESTANE® 58881 Ether Based Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Ether Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® 58881 Ether Based Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Very high tensile strength, excellent low temperature flexibility, and superior abrasion and cut resistanceUses: Extrusion – Wire and cable, Hose and tube & General purposeAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Maximum Moisture Content 0.020
0.020
Mechanical Properties Metric English Comments
Hardness, Shore A 77 - 83

@Time 5.00 sec
77 - 83

@Time 0.00139 hour
ASTM D2240
Tensile Strength 23.4 MPa
3390 psi
ASTM D412
Elongation at Break 710 %
710 %
ASTM D412
100% Modulus 0.00480 GPa
0.696 ksi
ASTM D412
300% Modulus 0.00680 GPa
0.986 ksi
ASTM D412
Flexural Modulus 0.0171 GPa
2.48 ksi
ASTM D790
Tear Strength 17.5 kN/m
100 pli
Trouser; ASTM D470
Graves Tear Strength 55.2 kN/m
315 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 3.0
3.0
CS-17, 1000g; ASTM D3389 B
Compression Set 18 %

@Temperature 23.0 °C,
Time 79200 sec
18 %

@Temperature 73.4 °F,
Time 22.0 hour
61 %

@Temperature 70.0 °C,
Time 79200 sec
61 %

@Temperature 158 °F,
Time 22.0 hour
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -52.0 °C
-61.6 °F
DSC
Processing Properties Metric English Comments
Zone 1 177 °C
351 °F
Extrusion
Zone 2 182 °C
360 °F
Extrusion
Zone 3 188 °C
370 °F
Extrusion
Zone 4 191 °C
376 °F
Extrusion
Adapter Temperature 191 °C
376 °F
5, Extrusion
Die Temperature 185 °C
365 °F
Zone 2, Extrusion
191 °C
376 °F
6, Zone 1, Extrusion
Drying Temperature 104 °C
219 °F
DSC
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Dew Point -40.0 °C
-40.0 °F