Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol ESTANE® ETE60DS3 Ester Based Thermoplastic Polyurethane (European Grade)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Polyester Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® ETE60DS3 Ester Based Thermoplastic Polyurethane (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability in a flexible thermoplastic elastomer system that is easy to process in a wide range of equipment. The Estane® TPU portfolio of products offers high performance polyester - and polyether - based resins and compounds in a broad range of hardnesses to meet a variety of application needs.Benefits of Estane® TPU: Outstanding Abrasion and Wear ResistanceExcellent Low Temperature FlexibilitySuperior Toughness and DurabilityEase of Processing and Manufacturing FlexibilityColorability and Paintability with no adhesion promoterApplications: Film & SheetFabric coating & melt coatingWire & CableHose, Tube & ProfileCustom moldingCustom compoundingAutomotive interior/chassis and exterior painted trimSpecific Notes for this Material: Easy to extrude technology Information provided by Noveon, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
DIN 53479
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
DIN 53505
Tensile Strength, Ultimate 43.0 MPa
6240 psi
DIN 53504
Elongation at Break 470 %
470 %
DIN 53504
50% Modulus 0.0161 GPa
2.34 ksi
DIN 53504
100% Modulus 0.0176 GPa
2.55 ksi
DIN 53504
300% Modulus 0.0275 GPa
3.99 ksi
DIN 53504
Flexural Stiffness 177.00 MPa
25672 psi
ASTM D747
Tear Strength 150 kN/m
856 pli
DIN 53515
Abrasion 63
63
mm<sup>3</sup>; DIN 53516
Thermal Properties Metric English Comments
Vicat Softening Point 95.0 °C
203 °F
A50; DIN 53460
Descriptive Properties Value Comments
E-Modulus 130 mm/min