Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Estaloc® 61225 Polyester-Type Thermoplastic Alloy

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTALOC®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Estaloc® 61225 Polyester-Type Thermoplastic Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type: Estaloc® 61225 Alloy RETPU is a polyester-type thermoplastic alloy.Features: Fast cycling, dimensional stability, durability, aesthetics, low temperature impact.Uses: Injection molding.Availability: Americas, Europe, Middle East, Africa, India and AsiaInformation Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
Maximum Moisture Content 0.020
0.020
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
flex bar; ASTM D955
0.0050 cm/cm
0.0050 in/in
disc; ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore D 61 - 67

@Time 5.00 sec
61 - 67

@Time 0.00139 hour
ASTM D2240
Tensile Strength, Ultimate 32.0 MPa
4640 psi
ASTM D638
Elongation at Break 180 %
180 %
ASTM D638
Tensile Modulus 1.03 GPa
149 ksi
ASTM D638
Flexural Strength 28.0 MPa
4060 psi
ASTM D790
Flexural Modulus 0.830 GPa
120 ksi
ASTM D790
Izod Impact, Notched 0.640 J/cm

@Temperature -40.0 °C
1.20 ft-lb/in

@Temperature -40.0 °F
ASTM D256
9.60 J/cm

@Temperature 23.0 °C
18.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 69.0 °C
156 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 57.0 °C
135 °F
ASTM D648
Processing Properties Metric English Comments
Rear Barrel Temperature 221 °C
430 °F
Middle Barrel Temperature 226 °C
439 °F
Front Barrel Temperature 226 °C
439 °F
Nozzle Temperature 232 °C
450 °F
Melt Temperature 232 °C
450 °F
Drying Temperature 104 °C
219 °F
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Dew Point -40.0 °C
-40.0 °F
Injection Pressure 69.0 - 103 MPa
10000 - 14900 psi
69.0 - 103 MPa
10000 - 14900 psi
Hold Pressure 35.0 - 69.0 MPa
5080 - 10000 psi
35.0 - 69.0 MPa
5080 - 10000 psi
Back Pressure 0.345 MPa
50.0 psi
0.345 MPa
50.0 psi
Screw Speed 30 - 80 rpm
30 - 80 rpm
30 - 80 rpm
30 - 80 rpm