Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Estane® 54601 Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Estane® 54601 Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Feature: Produces high coating weight in one pass at high production speed. Broad process window and transparent spherical pellets.Uses: Melt roll coated fabrics and unsupported foilsAvailable in Americas, Europe, Middle East, Africa and IndiaInformation Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ISO 2781
Maximum Moisture Content 0.10
0.10
Melt Flow 45 - 65 g/10 min

@Load 8.70 kg,
Temperature 190 °C
45 - 65 g/10 min

@Load 19.2 lb,
Temperature 374 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 93

@Time 5.00 sec
93

@Time 0.00139 hour
ISO 868
Tensile Strength 44.0 MPa
6380 psi
ISO 527-3/5/500
Elongation at Break 580 %
580 %
50% Modulus 0.00780 GPa
1.13 ksi
100% Modulus 0.00850 GPa
1.23 ksi
300% Modulus 0.0140 GPa
2.03 ksi
Tear Strength 81.0 kN/m
462 pli
ISO 34B
Abrasion 48
48
[mm<sup>3</sup>]
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Processing Properties Metric English Comments
Zone 1 180 °C
356 °F
Zone 2 180 °C
356 °F
Zone 3 175 °C
347 °F
Zone 4 175 °C
347 °F
Adapter Temperature 170 °C
338 °F
5
Die Temperature 170 °C
338 °F
6
Roll Temperature 160 °C
320 °F
1
170 °C
338 °F
2
Drying Temperature 90.0 °C
194 °F
Dry Time 3.00 hour
3.00 hour
Dew Point -40.0 - -30.0 °C
-40.0 - -22.0 °F