Lubrizol Estane® ALR CL57D Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Estane® ALR CL57D Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type: Estane® ALR CL570 is an aliphatic, polycaprolactone-based TPU with a Shore D Durometer of 57.Features: Contains a UV package that enhances outdoor weatherability. This high performance resin is clear, UV resistant; it will not discolor and has excellent mechanical properties.Uses: Outdoor applications, protective films and graphics.Available in Americas, Europe, Middle East, Africa, India and AsiaInformation Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Melt Flow 3.2 g/10 min

@Load 2.16 kg,
Temperature 175 °C
3.2 g/10 min

@Load 4.76 lb,
Temperature 347 °F
ASTM D1230
Mechanical Properties Metric English Comments
Hardness, Shore D 57

@Time 5.00 sec
57

@Time 0.00139 hour
ASTM D2240
Tensile Strength, Ultimate 64.5 MPa
9350 psi
ASTM D412
Elongation at Break 370 %
370 %
ASTM D412
100% Modulus 0.01507 GPa
2.185 ksi
ASTM D412
300% Modulus 0.02596 GPa
3.765 ksi
ASTM D412
Flexural Modulus 0.0634 GPa
9.20 ksi
ASTM D790
Processing Properties Metric English Comments
Zone 1 170 °C
338 °F
Extrusion
Zone 2 175 °C
347 °F
Extrusion
Zone 3 180 °C
356 °F
Extrusion
Zone 4 185 °C
365 °F
Extrusion
Die Temperature 185 °C
365 °F
Extrusion
Melt Temperature 185 °C
365 °F
Extrusion