Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Estane® ALR CL60D Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Estane® ALR CL60D Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type: Estane® ALR CL600 is a Shore D thermoplastic polyurethane (TPU) resin.Features: Contains a UV package that enhances outdoor weatherability, but does not contain lubricants or wax processing aids.Uses: Outdoor applicationsInformation Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Melt Flow 3.2 g/10 min

@Load 2.16 kg,
Temperature 175 °C
3.2 g/10 min

@Load 4.76 lb,
Temperature 347 °F
ASTM D1230
Mechanical Properties Metric English Comments
Hardness, Shore D 57
57
ASTM D2240
Tensile Strength, Ultimate 64.5 MPa
9350 psi
ASTM D412
Tensile Strength, Yield 15.07 MPa
2185 psi
at 100%; ASTM D412
25.96 MPa
3765 psi
at 200%; ASTM D412
Elongation at Break 370 %
370 %
ASTM D412
Flexural Modulus 0.0634 GPa
9.20 ksi
ASTM D790
Processing Properties Metric English Comments
Feed Temperature 175 °C
347 °F
Middle Barrel Temperature 180 °C
356 °F
Nozzle Temperature 185 °C
365 °F
Melt Temperature 185 °C
365 °F