Lubrizol Estane® ALR E68D-V Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Estane® ALR E68D-V Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type: Estane® ALR E68D-V is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Available in AmericasInformation Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore D 67
67
ASTM D2240
Tensile Strength, Ultimate 55.8 MPa
8100 psi
ASTM D412
Elongation at Break 310 %
310 %
ASTM D412
100% Modulus 0.0234 GPa
3.40 ksi
ASTM D412
200% Modulus 0.0331 GPa
4.80 ksi
ASTM D412
300% Modulus 0.0490 GPa
7.10 ksi
ASTM D412
Flexural Modulus 0.634 GPa
92.0 ksi
ASTM D790