Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Estane® ETE 55DS3 Thermoplastic Polyurethane, Easy-to-Extrude

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Estane® ETE 55DS3 Thermoplastic Polyurethane, Easy-to-Extrude.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type: Estane® ETE 55DS3 is a 55D aromatic polyester-based thermoplastic polyurethane (TPU).Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, high transparency, excellent chemical resistance.Uses: Extrusion: Hose and Tube, Profile. Injection molding: Various.Available in Americas, Europe, Middle East, Africa, India and AsiaInformation Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
ASTM D792
Maximum Moisture Content 0.020
0.020
Mechanical Properties Metric English Comments
Hardness, Shore D 52 - 58

@Time 5.00 sec
52 - 58

@Time 0.00139 hour
ASTM D2240
Tensile Strength 71.0 MPa
10300 psi
ASTM D412
Elongation at Break 440 %
440 %
ASTM D412
100% Modulus 0.0145 GPa
2.10 ksi
ASTM D412
300% Modulus 0.0331 GPa
4.80 ksi
ASTM D412
Tear Strength 35.9 kN/m
205 pli
Trouser; ASTM D470
Graves Tear Strength 154 kN/m
880 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 58

@Load 1.00 kg
58

@Load 2.20 lb
H-18 wheel; ASTM D3389
Thermal Properties Metric English Comments
Melting Point 180 °C
356 °F
DSC
Glass Transition Temp, Tg -39.0 °C
-38.2 °F
DSC
Processing Properties Metric English Comments
Zone 1 199 °C
390 °F
Extrusion
Zone 2 204 °C
399 °F
Extrusion
Zone 3 204 °C
399 °F
Extrusion
Zone 4 210 °C
410 °F
Extrusion
Adapter Temperature 213 °C
415 °F
5, Extrusion
Die Temperature 210 °C
410 °F
6, Zone 1, Extrusion
210 °C
410 °F
Zone 2, Extrusion
Drying Temperature 104 °C
219 °F
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Dew Point -40.0 °C
-40.0 °F