Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Estane® X-590A-2FR Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type: Estane® X-590A-2FR TPU is a Shore 89A, polyester type thermoplastic polyurethane elastomer.Uses: Film Blowing, Extrusion.Available in AsiaInformation Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 89
89
ASTM D2240
Tensile Strength, Ultimate 34.3 MPa
4980 psi
ASTM D412
Tensile Strength, Yield 7.85 MPa
1140 psi
at 100% elongation; ASTM D412
14.7 MPa
2130 psi
at 300% elongation; ASTM D412
Elongation at Break 650 %
650 %
ASTM D412
Tear Strength 103 kN/m
588 pli
Die C; ASTM D624
Compression Set 25 %

@Temperature 23.0 °C,
Time 79200 sec
25 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
55 %

@Temperature 70.0 °C,
Time 79200 sec
55 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395
Thermal Properties Metric English Comments
Vicat Softening Point 90.0 °C
194 °F
ASTM D1525
Processing Properties Metric English Comments
Zone 1 180 °C
356 °F
Zone 2 185 °C
365 °F
Zone 3 190 °C
374 °F
Zone 4 190 °C
374 °F
Die Temperature 185 °C
365 °F
Descriptive Properties Value Comments
Adaptor (°C) 195