Lubrizol Hipscon™ M-505 Static Control High Impact Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Lubrizol (former Noveon)
Trade Name Hipscon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Hipscon™ M-505 Static Control High Impact Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hipscon™ M-505 is a conductive, carbon black filled, High Impact Polystyrene available as extruded sheet. Thermoformed trays are lightweight and easily formed into deep pockets that maintain uniform static protection. Hipscon maintains extremely low gloss surfaces after forming, allowing for easy reading of package contents via automated sensors. Hipscon™ M-505 sheet is available in custom extruded gauges from 0.012 to 0.080 inch and widths of 10 to 48 inches. Product is typically provided as rollstock with a smooth surface finish. Features:Hipscon M-505 Chloride free(
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 17.9 MPa
2600 psi
ASTM D638
Elongation at Break 1.3 %
1.3 %
ASTM D638
Flexural Modulus 1.59 GPa
230 ksi
ASTM D790-92
Tear Strength 68.0 kN/m
388 pli
ASTM D646
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
ASTM D648
Optical Properties Metric English Comments
Gloss 9.0 %
9.0 %
60°; Front
14 %
14 %
60°; Back
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+7 ohm-cm
1.00e+7 ohm-cm
ASTM D257
Surface Resistivity per Square 1e+05
1e+05
50% RH; ASTM D257
Static Decay <= 0.010 sec
<= 0.010 sec
FTMS-101C; 12% R.H., (+5000 V to 50 V)
<= 0.010 sec
<= 0.010 sec
FTMS-101C; 12% R.H., (-5000 V to -50 V)
Descriptive Properties Value Comments
Color Black