Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Telene 1620 A/BK Dicyclopentadiene (DCPD)

Category Polymer , Thermoset , Polydicyclopentadiene (PDCPD)
Manufacturer Lubrizol (former Noveon)
Trade Name Telene
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Telene 1620 A/BK Dicyclopentadiene (DCPD).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Telene® is a two-component system based on extra-high purity dicyclopentadiene (DCPD). Telene® is processed using a standard high-pressure RIM Equipment (Reaction Injection Molding). Telene® results in a polymer showing a unique combination of stiffness and high impact resistance, as well as good thermal properties. Telene® is self-demolding without any need for release agents.Information provided by Noveon, Inc.
Physical Properties Metric English Comments
Viscosity 1000 cP
1000 cP
265 sec; Calculated
Brookfield Viscosity 210 - 290 cP

@Temperature 30.0 °C
210 - 290 cP

@Temperature 86.0 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 44.0 MPa
6380 psi
ISO 527
Flexural Strength 67.0 MPa
9720 psi
ISO 1783
Flexural Modulus 1.85 GPa
268 ksi
ISO 178
Izod Impact, Notched (ISO) 22.0 kJ/m²
10.5 ft-lb/in²
ASTM D 256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air >= 180 °C
>= 356 °F
Exotherm Temp; Method 4
Deflection Temperature at 1.8 MPa (264 psi) 112 °C
234 °F
ASTM D 648
Smoke Density 1.5 - 1.83 min
1.5 - 1.83 min
At 30°C; Method 4
Processing Properties Metric English Comments
Processing Temperature 60.0 °C
140 °F
non show side
80.0 °C
176 °F
show side
Users viewing this material also viewed the following: