Material Notes:
Silvaloy A30 does not contain cadmium and is often used as an alternate to cadmium containing alloys when the brazed assembly comes in contact with food or dairy products. Its slightly higher melt temperature provides improved mechanical strengths when exposed to elevated temperatures. It is used extensively in joining copper, brass, nickel, silvers, and ferrous alloys. Typical applications are the joining of ferrous, nonferrous, and dissimilar metals and alloys with close joint clearances.Information provided by Lucas-Milhaupt Warwick, LLC (formerly Wolverine Joining Technologies).
Physical Properties Metric English Comments
Specific Gravity 8.85 g/cc
8.85 g/cc
Density 8.84 g/cc
0.319 lb/in³
Thermal Properties Metric English Comments
Melting Point 677 - 766 °C
1250 - 1410 °F
Solidus 677 °C
1250 °F
Liquidus 766 °C
1410 °F
Maximum Service Temperature, Air 204 °C
400 °F
continuous
316 °C
600 °F
intermittent
Component Elements Properties Metric English Comments
Copper, Cu 37 - 39 %
37 - 39 %
Other, total <= 0.15 %
<= 0.15 %
Silver, Ag 29 - 31 %
29 - 31 %
Zinc, Zn 30 - 34 %
30 - 34 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000707 ohm-cm
0.00000707 ohm-cm
Processing Properties Metric English Comments
Processing Temperature 766 - 857.2 °C
1410 - 1575 °F
Brazing Temperature
Descriptive Properties Value Comments
Color Light Yellow
Electrical Conductivity (% IACS) 24.4