Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lucent Polymers GPC-0202 20 Polycarbonate, Glass Reinforced, Injection Grade

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 20% Glass Filled
Manufacturer Lucent Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucent Polymers GPC-0202 20 Polycarbonate, Glass Reinforced, Injection Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Recycled ContentAdd "R" for Added ReleaseAdd "U" for UV StabilizedInformation provided by Lucent Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0030 cm/cm

@Thickness 3.17 mm
0.0030 in/in

@Thickness 0.125 in
1/8" Section
Mechanical Properties Metric English Comments
Tensile Strength, Yield 96.55 MPa
14000 psi
ASTM D638
Elongation at Break >= 4.0 %
>= 4.0 %
ASTM D638
Flexural Strength 151.72 MPa
22005 psi
ASTM D790
Flexural Modulus 5.517 GPa
800.2 ksi
ASTM D790
Izod Impact, Notched 1.335 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
2.501 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 140.56 °C
285.01 °F
ASTM D648