Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lucent Polymers PC/PET-1515 Polycarbonate+PET, General Purpose, Injection Grade

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/PET Polyester Blend , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer Lucent Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucent Polymers PC/PET-1515 Polycarbonate+PET, General Purpose, Injection Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0080 cm/cm

@Thickness 3.17 mm
0.0080 in/in

@Thickness 0.125 in
1/8" Section
Melt Flow 15 g/10 min

@Load 5.00 kg,
Temperature 260 °C
15 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.17 MPa
8002 psi
ASTM D638
Elongation at Break >= 118 %
>= 118 %
ASTM D638
Flexural Strength 84.83 MPa
12300 psi
ASTM D790
Flexural Modulus 2.2069 GPa
320.08 ksi
ASTM D790
Izod Impact, Notched 8.01 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
15.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 121.11 °C
250.00 °F
ASTM D648