Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lucite International Colacryl ® TS1304 Acrylic Solution Resin

Category Polymer , Thermoplastic , Acrylic (PMMA)
Manufacturer Lucite International
Trade Name Colacryl ®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucite International Colacryl ® TS1304 Acrylic Solution Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Colacryl® TS1304 is a soft resin based on n-butyl methacrylate. This resin is aimed at applications requiring high flexibility and good burn-out properties, supplied in a heavy petroleum action. It is compatible with most common plasticisers and some other resin types.Applications: ceramic covercoats, screen printing mediaInformation provided by Lucite International
Physical Properties Metric English Comments
Solids Content 50 %
50 %
Viscosity 9000 cP
9000 cP
Thermal Properties Metric English Comments
Flash Point 65.0 °C
149 °F
Chemical Properties Metric English Comments
Total Acid Number 0.00
0.00
Descriptive Properties Value Comments
Solvent Solvesso 150