Lucite International Diakon® ST50G8 Toughened Acrylic Polymer

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, Impact Modified, Molded
Manufacturer Lucite International
Trade Name Diakon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucite International Diakon® ST50G8 Toughened Acrylic Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed by injection molding or extrusion.Information provided by Lucite International
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
Water Absorption 0.37 %
0.37 %
ISO 62
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
Melt Flow 0.90 g/10 min
0.90 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell M 25
25
ISO 2039-2
Tensile Strength 43.0 MPa
6240 psi
ISO 527
Elongation at Break 40 %
40 %
ISO 527
Flexural Strength 50.0 MPa
7250 psi
ISO 178
Flexural Modulus 1.50 GPa
218 ksi
ISO 178
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
ISO 180/1A
Charpy Impact Unnotched 8.00 J/cm²
38.1 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.850 J/cm²
4.04 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear 120 µm/m-°C
66.7 µin/in-°F
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 91.0 °C
196 °F
ISO 75A
Vicat Softening Point 92.0 °C
198 °F
ISO 306B
107 °C
225 °F
ISO 306A
Flammability, UL94 HB
HB
Glow Wire Test 650 °C
1200 °F
IEC 695-2-1
Optical Properties Metric English Comments
Refractive Index 1.49
1.49
ISO 489
Haze 3.0 %
3.0 %
ASTM D1003
Transmission, Visible 89 %
89 %
ASTM D1003