Lucite International Elvacite ® 2008 Acrylic Resin

Category Polymer , Thermoplastic , Acrylic (PMMA)
Manufacturer Lucite International
Trade Name Elvacite ®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucite International Elvacite ® 2008 Acrylic Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Elvacite® 2008 is a low molecular weight methyl methacrylate copolymer. It is used in lacquers and gravure inks requiring low viscosity at high solids. 2008 provides good activity for pigment dispersions.Applications: laquer coatings, vinyl topcoats, gravure inksInformation provided by Lucite International
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
Particle Size 140 - 240 µm
140 - 240 µm
Viscosity Measurement 0.172 - 0.194
0.172 - 0.194
Inherent viscosity, 0.25 g polymer in 50 ml of methylene chloride; No. 50 Cannon-Fenske viscometer.
Molecular Weight 37000 g/mol
37000 g/mol
Mechanical Properties Metric English Comments
Elongation at Break 0.50 %
0.50 %
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 105 °C
221 °F
Chemical Properties Metric English Comments
Total Acid Number 9.0
9.0
Processing Properties Metric English Comments
Moisture Content 0.50 %
0.50 %