Material Notes:
Elvacite® 2021 is a high molecular weight methyl methacrylate polymer. It is used in barrier coatings for vinyl. Its high molecular weight provides excellent abrasion resistance.Information provided by Lucite International
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
Particle Size 110 - 230 µm
110 - 230 µm
Viscosity Measurement 0.469 - 0.527
0.469 - 0.527
Inherent viscosity, 0.25 g polymer in 50 ml of methylene chloride; No. 50 Cannon-Fenske viscometer.
Molecular Weight 119000 g/mol
119000 g/mol
Mechanical Properties Metric English Comments
Tensile Strength 103 MPa
14900 psi
Elongation at Break 4.0 %
4.0 %
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 95.0 °C
203 °F
Chemical Properties Metric English Comments
Total Acid Number 0.00
0.00
Processing Properties Metric English Comments
Moisture Content 0.50 %
0.50 %