Lucite International Elvacite ® 2021E Acrylic Resin

Category Polymer , Thermoplastic , Acrylic (PMMA)
Manufacturer Lucite International
Trade Name Elvacite ®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucite International Elvacite ® 2021E Acrylic Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Elvacite® 2021E is a high molecular weight methyl methacrylate. It provides a balance of solubility and hardness. It is used in migration barrier top coating for vinyl substrates. It is also used to give tough films on many other plastic substrates. Elvacite 2021E complies with the compositional requirements of the following FDA Regulations in relation to food contact: 21 CFR 175.105, 175.300, 175.320*, 176.170, 176.180, and 177.1010Information provided by Lucite International
Physical Properties Metric English Comments
Viscosity Measurement 0.46 - 0.53
0.46 - 0.53
Inherent viscosity, 0.25 g polymer in 50 ml of methylene chloride; No. 50 Cannon-Fenske viscometer.
Molecular Weight 119000 g/mol
119000 g/mol
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 95.0 °C
203 °F
Chemical Properties Metric English Comments
Total Acid Number 0.00
0.00
Processing Properties Metric English Comments
Moisture Content 0.50 %
0.50 %