Lucite International Elvacite ® 2550 Acrylic Resin

Category Polymer , Thermoplastic , Acrylic (PMMA)
Manufacturer Lucite International
Trade Name Elvacite ®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucite International Elvacite ® 2550 Acrylic Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Elvacite® 2550 is a solid bead methacrylate copolymer resin. It is designed to provide excellent adhesion to metal surfaces and is a resin with good flexibility and medium molecular weight. As such, it has found use in staple cement formulations. Since Elvacite® 2550 is an all methacrylate resin, resistance to ultraviolet degradation with good exterior durability is expected.Information provided by Lucite International
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
Density 1.043 g/cc
0.03768 lb/in³
Brookfield Viscosity 2200 cP

@Temperature 25.0 °C
2200 cP

@Temperature 77.0 °F
in Toluene, 37.5% solids
3600 cP

@Temperature 25.0 °C
3600 cP

@Temperature 77.0 °F
in Toluene, 40.0% solids
Viscosity Measurement 0.32
0.32
Inherent viscosity, 0.25 g polymer in 50 ml of methylene chloride; No. 50 Cannon-Fenske viscometer.
Molecular Weight 98000 g/mol
98000 g/mol
Mechanical Properties Metric English Comments
Hardness, Knoop 3.5
3.5
Tukon Hardness
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 36.0 °C
96.8 °F
Chemical Properties Metric English Comments
Total Acid Number 17
17