Material Notes:
Elvacite® 4402 is a solid methyl methacrylate copolymer bead resin designed for use in formulating environmentally sound thermosetting coatings and adhesives. The resin may be used as the main binder in acrylic systems, or blended with other resins to improve weather resistance and clarity.Information provided by Lucite International
Physical Properties Metric English Comments
Viscosity Measurement 0.16
0.16
Inherent viscosity, 0.25 g polymer in 50 ml of methylene chloride; No. 50 Cannon-Fenske viscometer.
Molecular Weight 40000 g/mol
40000 g/mol
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 76.0 °C
169 °F
Chemical Properties Metric English Comments
Total Acid Number 5.0
5.0
Descriptive Properties Value Comments
Hydroxyl Number 9