Lucobit Lucocell® FG3000 Cellulose Asphalt Additive

Category Polymer , Thermoplastic , Cellulosic
Manufacturer Lucobit AG
Trade Name Lucocell®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucobit Lucocell® FG3000 Cellulose Asphalt Additive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lucocell® FG3000 micro grains – cellulose additives for SMA –Stone Mastic Asphalt or Split Mastic Asphalt, which is used as finish for all road types. Due to their 3D structure, cellulose fibers maintain a comparatively high viscosity of bitumen, thus preventing its seepage and formation of asphalt mix segregation at high temperatures during storage, transport and SMA placing. At the same time they enable creation of a thicker bitumen layer around each rock particle, thus preventing oxidation, moisture penetration and lifting or cracking of the aggregate. Because of the nature of the product cellulose fibers may not be exposed to water and mix temperatures higher than 200°C.Information provided by Lucobit AG
Physical Properties Metric English Comments
Apparent Bulk Density 0.450 g/cc
0.0163 lb/in³
Descriptive Properties Value Comments
Average Fiber Diameter, µm 45
Average Fiber Length, µm 1100