Lucobit Lucofin® 1400HN Powder Ethylene Butyl Acrylate

Category Polymer , Thermoplastic , Ethylene Butyl Acrylate
Manufacturer Lucobit AG
Trade Name Lucofin®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucobit Lucofin® 1400HN Powder Ethylene Butyl Acrylate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lucofin 1400HN Powder is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400HN Powder is softer and more flexible than ethylene homopolymers with comparable density.Applications:• Supporting material for compounds• Polymer modification of bitumen and asphalt• Powder coatingInformation provided by Lucobit AG
Physical Properties Metric English Comments
Density 0.921 g/cc
0.0333 lb/in³
ISO 1183
Melt Flow 0.25 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.25 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength 27.0 MPa
3920 psi
MD; ISO 527
29.0 MPa
4210 psi
TD; ISO 527
Tensile Strength, Yield 6.70 MPa
972 psi
ISO 527
Elongation at Break 450 %
450 %
MD; ISO 527
600 %
600 %
TD; ISO 527
Tensile Modulus 0.144 GPa
20.9 ksi
ISO 527
Thermal Properties Metric English Comments
Melting Point 102 °C
216 °F
ISO 3146
Vicat Softening Point 86.0 °C
187 °F
ISO 306
Processing Properties Metric English Comments
Processing Temperature 160 - 240 °C
320 - 464 °F
Bitumen modification
160 - 270 °C
320 - 518 °F
Coatings
160 - 290 °C
320 - 554 °F
Compounding
Descriptive Properties Value Comments
Comonomer BA 0.09
Failure Energy, J/mm 21