Material Notes:
Lucofin 1400MN is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400MN is softer and more flexible than ethylene homopolymers with comparable density. Lucofin 1400MN is used primarily for injection applications, but is also suited for extrusion purposes.Information provided by Lucobit AG
Physical Properties Metric English Comments
Density 0.924 g/cc
0.0334 lb/in³
ISO 1183
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 88
88
ISO 868
Hardness, Shore D 32
32
ISO 868
Tensile Strength, Yield 3.50 MPa
508 psi
ISO 527
Elongation at Yield 13 %
13 %
ISO 527
Modulus of Elasticity 0.0450 GPa
6.53 ksi
ISO 527
Thermal Properties Metric English Comments
Melting Point 95.0 °C
203 °F
ISO 3146
Vicat Softening Point 60.0 °C
140 °F
ISO 306
Processing Properties Metric English Comments
Processing Temperature 160 - 190 °C
320 - 374 °F
Profiles and hoses
160 - 190 °C
320 - 374 °F
Blow molding
160 - 190 °C
320 - 374 °F
Blown film
160 - 230 °C
320 - 446 °F
Flat-sheet
160 - 270 °C
320 - 518 °F
Coatings
Melt Temperature 180 - 250 °C
356 - 482 °F
Mold Temperature 10.0 - 40.0 °C
50.0 - 104 °F
Descriptive Properties Value Comments
Comonomer BA 0.17
DIN 51451