Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lushan Solar EVA Film Lamination, Low Temperature Ultra Fast Cure

Category Polymer , Film , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
Manufacturer Lushan
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lushan Solar EVA Film Lamination, Low Temperature Ultra Fast Cure.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cure solar EVA film has developed to be a stable, high properties, and reputable products, and widely used in China and overseas market. Lushan ultra fast cure solar EVA film has very good processing properties that helps PV module manufactures with the most effective production way and save the cost as much as possible.Information provided by Lushan
Processing Properties Metric English Comments
Gel Time 0.000 min

@Temperature 136 °C
0.000 min

@Temperature 277 °F
0% Gel content
0.000 min

@Temperature 138 °C
0.000 min

@Temperature 280 °F
0% Gel content
0.000 min

@Temperature 140 °C
0.000 min

@Temperature 284 °F
4.42% Gel content
0.000 min

@Temperature 143 °C
0.000 min

@Temperature 289 °F
47.33% Gel content
0.000 min

@Temperature 145 °C
0.000 min

@Temperature 293 °F
51.3% Gel content
2.00 min

@Temperature 136 °C
2.00 min

@Temperature 277 °F
15.17% Gel content
2.00 min

@Temperature 138 °C
2.00 min

@Temperature 280 °F
27.49% Gel content
2.00 min

@Temperature 140 °C
2.00 min

@Temperature 284 °F
37.24% Gel content
2.00 min

@Temperature 143 °C
2.00 min

@Temperature 289 °F
74.31% Gel content
2.00 min

@Temperature 145 °C
2.00 min

@Temperature 293 °F
80.43% Gel content
4.00 min

@Temperature 136 °C
4.00 min

@Temperature 277 °F
53.78% Gel content
4.00 min

@Temperature 138 °C
4.00 min

@Temperature 280 °F
70..21% Gel content
4.00 min

@Temperature 140 °C
4.00 min

@Temperature 284 °F
71.67% Gel content
4.00 min

@Temperature 143 °C
4.00 min

@Temperature 289 °F
82.43% Gel content
4.00 min

@Temperature 145 °C
4.00 min

@Temperature 293 °F
85.67% Gel content
6.00 min

@Temperature 136 °C
6.00 min

@Temperature 277 °F
74.06% Gel content
6.00 min

@Temperature 138 °C
6.00 min

@Temperature 280 °F
79.24% Gel content
6.00 min

@Temperature 140 °C
6.00 min

@Temperature 284 °F
83.45% Gel content
6.00 min

@Temperature 143 °C
6.00 min

@Temperature 289 °F
85.68% Gel content
6.00 min

@Temperature 145 °C
6.00 min

@Temperature 293 °F
88.61% Gel content
8.00 min

@Temperature 136 °C
8.00 min

@Temperature 277 °F
80.39% Gel content
8.00 min

@Temperature 138 °C
8.00 min

@Temperature 280 °F
83.56% Gel content
8.00 min

@Temperature 140 °C
8.00 min

@Temperature 284 °F
84.78% Gel content
8.00 min

@Temperature 143 °C
8.00 min

@Temperature 289 °F
87.59% Gel content
8.00 min

@Temperature 145 °C
8.00 min

@Temperature 293 °F
89.23% Gel content
10.0 min

@Temperature 136 °C
10.0 min

@Temperature 277 °F
82.79% Gel content
10.0 min

@Temperature 138 °C
10.0 min

@Temperature 280 °F
87.03% Gel content
10.0 min

@Temperature 140 °C
10.0 min

@Temperature 284 °F
86.21% Gel content
10.0 min

@Temperature 143 °C
10.0 min

@Temperature 289 °F
89.93% Gel content
10.0 min

@Temperature 145 °C
10.0 min

@Temperature 293 °F
90.34% Gel content
Users viewing this material also viewed the following: