Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Adflexâ„¢ Q 200 F Polyolefin

Category Polymer , Film , Thermoplastic , Polyolefin , Polyolefin, Film Grade , Polyolefin, Film Grade (Polyolefin)
Manufacturer LyondellBasell
Trade Name Adflex™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Adflexâ„¢ Q 200 F Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Adflexâ„¢ Q 200 F fractional melt flow, low modulus thermoplastic olefin (TPO) resin is designed for extrusion applications. It is based on material produced from Basell's proprietary "Catalloy" process. This resin is ideal for making soft hygienic or heavy duty films. It can also be used to modify LDPE or LLDPE resins in order to improve mechanical characteristics, puncture resistance and to allow further downgauging. It contains no slip or antiblock. Q 200 F resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, except for certain fatty foods. Uses: Film, automotive applicationsInformation provided by Basell.
Physical Properties Metric English Comments
Density 0.882 g/cc
0.0319 lb/in³
ASTM D792
Melt Flow 0.80 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.80 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 48
48
ASTM D2240
Tensile Strength, Yield 7.58 MPa
1100 psi
ASTM D 638
Elongation at Break 350 %
350 %
ASTM D 638
Elongation at Yield 18 %
18 %
ASTM D 638
Flexural Modulus 0.152 GPa
22.0 ksi
1% Secant, Procedure A; ASTM D790
Izod Impact, Notched NB
NB
73°F; ASTM D256